2008 · 32 citations · 0 references
EngineeringMaterials EngineeringMaterials ScienceBuilding MaterialsMaterials CharacterizationPavement EngineeringAsphalt MaterialsPavement DesignPavement MaterialsPavement Performance AnalysisPaving MaterialsAsphalt BinderAsphalt MixturesElemental Sulfur ChemistryModifier EffectsRubber-modified AsphaltRubberized AsphaltStorage Stability EvaluationVulcanization
The use of tire rubber (TR) as an asphalt modifier to improve the asphalt mixture performance has been succeeded. Because the poor compatibility between TR and asphalt the storage stability of TR modifier is a main concern. The main objective of this study is to enhance the properties of tire rubber modified asphalt binder and improve the storage stability through the addition of Styrene-Butadiene-Styrene (SBS) and elemental sulfur (S). Low quality asphalt paving 60/70 penetration grade was modified with 2, 3, 4, and5% TR (by asphalt wt.) and equal parts of SBS and TR at 2, 3, 4 and5% by asphalt wt. were also prepared before and after the addition of sulfur. Physical properties including softening point penetration at 25°C and ductility at 4°C , penetration temperature susceptibility (PTS) and penetration index (PI) of modified binders were examined. The storage stability of modified and unmodified asphalt were tested at 140,1160 and 200°C to detect the optimum and critical vulcanization temperature. The effect of TR modified asphalt binder on the asphalt mixture performance before and after the addition of either SBS or SBS/S were evaluated using Marshall stability and flow test. The effect of the vulcanized blend to resist plastic deformation of asphalt mixture was evaluated through wheel tracking test .Results indicated that PTS of modified asphalt before and after vulcanization was largely decreased. The storage stability of TR/SBS modified asphalt after vulcanization process has been achieved at 160°C while the critical degradation temperature reached to 200°C. Marshall Stability and resistance to plastic deformation of TR/SBS were increased after the addition of sulfur. The best improvements were obtained at 4% TR/SBS/ 1%S.