PubMed · 2001 · 32 citations · 17 references
DentistryMaterials EngineeringMaterials ScienceDental MaterialsMechanical Behavior Of MaterialsMechanical Properties Of Dental MaterialsCementitious MaterialsGlass Ionomer CementsMaterial PropertiesStrength Of MaterialsStrength PropertiesTensile PropertiesDiametral Tensile StrengthGlass Ionomer CompositesRestorative ApplicationsTensile StrengthTensile Strength Testing
The aim of this study was to analyze the diametral tensile strengths of three resin-modified restorative glass ionomer cements--Vitremer, Fuji II LC and Photac Fil and one compomer--Dyract. They were tested at 1 hour, 1 day and 1 week. Kratos testing machine was used to load the specimens at a cross-head speed of 0.5 mm/min. The data were analyzed by two-way ANOVA and Tukey's test that showed statistically significant differences among the materials. The tested materials presented an increase in strength from 1 hour to 1 week and were as follows for each material respectively: Vitremer (19.22-27.29), Fuji II LC (23.91-28.67), Photac Fil (19.35-22.86), Dyract (28.83-46.95). Dyract presented the highest strengths.
17