1991 · 39 citations · 7 references
Natural SciencesCivil EngineeringBuilding MaterialsInorganic ChemistryMineralogyCementitious MaterialsConcrete MaterialsMineral GenesisMineral LiberationSilicate MineralogySilicate MineralsMineralogical CompositionRock-forming MineralsSilica SolubilitySilicate Dissolution KineticsSilicate Mineral ChemistrySilicate Mineral StabilitySilicate StabilitySodium Hydroxide Electrolytes
The pH of the pore solution existing within concretes or lime-treated soils normally exceeds 12. When exposed to a solution witl a pH over 10, several rock-forming and soil-forming minerals are unstable, and dissolve with or without precipitation, depending on the nature and concentration of species in solution. In concrete, made with a typical cement containing 0.7a/o to l9o alkalis, after a few days, the composition of the liquid phase is dominated by sodium, potassium and hydroxide ions. In this study, the behavior of several common minerals in a pure sodium hydroxide solution was evaluated by the means of two experiments. First, mineral fragments were immersed in a lN NaOH solu-tion at 23oC for 265 days, then at 80oC for 7 days. The specimens were regularly analyzed with a SEM-EDX sys-tem. Secondly, the release of silica by silicate minerals in a lN NaOH solution was measured by means of the Chem-ical Method ASTM C 289 test (80'C, 24 hours). Of all rhe silicate minerals tested, the microcryslalline variety of sil-ica, chert, was the most unstable phase. Significant quan-tities of silica also were released by quartz and feldspars. Iron and magnesium silicates were found to be the mosr stable phases in the NaOH solution. Among the other minerals investigated, dolomite, siderite and gypsum are classified as highly reactive in the alkaline solution.
7