Science and Technology of Welding & Joining · 2004 · 142 citations · 5 references
Natural SciencesMaterials EngineeringMaterials ScienceMechanical Behavior Of MaterialsMetallic MaterialsMetallurgyAlloysDuctilityFracture ToughnessHeat-affected ZoneStainless SteelsSteel MaterialsGrain Size ReductionHeat Treatment EffectsHeat Treatment Effects On DuctilityMartensitic MicrostructureMartensitic Stainless SteelsMartensitic SteelsMicrostructureSteel Heat-affected Zone
The study investigates how non‑equilibrium δ‑ferrite affects the impact properties of supermartensitic stainless steel. The authors produced δ‑ferrite‑rich microstructures by high‑temperature furnace heat treatments and by Gleeble simulation to mimic weld heat‑affected zone conditions. Higher δ‑ferrite (≈14 %) raises the ductile‑to‑brittle transition temperature by ~50 °C, while reducing it to 2 % restores the transition to parent‑material levels; in simulated heat‑affected zones, δ‑ferrite has little effect on toughness and the DBTT remains comparable to the parent material.
The work presented in this paper focuses on the effect of the presence of non-equilibrium δ-ferrite on the impact properties of a supermartensitic stainless steel. To generate homogeneous δ-ferrite containing microstructures the material was, in the first part of the present study, subjected to a series of high temperature furnace heat treatments. Three microstructures possessing variable ferrite content and different grain sizes were generated. Charpy impact results indicate that the presence of 14% δ-ferrite in a martensitic matrix of 60 μm prior austenite grain size, raises the ductile to brittle transition temperature (DBTT) by about 50°C compared with a fully martensitic microstructure of 80 μm. For a similar grain size, reducing the amount of δ-ferrite from 14 to 2% restored the DBTT to a level comparable to that of the tempered parent material. A Gleeble simulator was used to create the range of microstructures found in a weld heat affected zone (HAZ). Testing of the simulated HAZ indicated that toughness was not significantly affected by the presence of δ-ferrite. The DBTT was comparable to that of the parent material and lower than that of the heat treated specimens containing 14% δ-ferrite.
5