Journal of the American Ceramic Society · 1989 · 165 citations · 6 references
Natural SciencesMaterials EngineeringMaterials ScienceCeramic MaterialsCeramicsMechanical Behavior Of MaterialsCeramic CompositesComposite MaterialsFiber PropertiesFiber-reinforced CompositesHigh-temperature MaterialsStructural CeramicsFibersHigh-temperature CeramicsHigh-temperature Mechanical BehaviorHigh-temperature StrengthMechanical Properties Of Ceramic CompositesOxide Ceramic CompositesThermomechanical Behavior Of CeramicsVoid Formation
Tensile strengths were measured and Young's moduli were estimated for two SiC‐based and three oxide ceramic fibers for temperatures from 25° to 1400°C. The SiC‐based fibers were stronger but less stiff than the oxide fibers at room temperature and retained more of both strength and stiffness to high temperatures. High‐temperature strengths of the SiC‐based fibers were limited by internal void formation and oxidation; those of the oxide fibers were limited by softening of an intergranular glassy phase.
6
Thermal stability of SiC fibres (Nicalon�)
T. Mah, Norman L. Hecht, Dale E. McCullum et al. · Journal of Materials Science · 1984 · 331 citations
Natural Sciences, Materials Engineering, Materials Science +14