Low‐Temperature Chemical Vapor Deposition Tungsten Carbide Coatings for Wear/Erosion Resistance

D. Garg, Paul N. Dyer, Duane Dimos, Swaminathan Sunder, H.E. Hintermann, M. Maillat

Journal of the American Ceramic Society · 1992 · 34 citations · 3 references

Concepts

Abstract

A new chemical vapor deposition (CVD) process has been developed to deposit hard coatings, containing tungsten carbide, at temperatures below 500°C. These coatings, which have been applied to both ferrous and nonferrous alloys, exhibit excellent resistance to wear and erosion. The coatings comprise a mixture of tungsten and the tungsten carbide, the latter being present as W 2 C, W 2 C + W 3 C, or W 3 C. The coatings' composition and properties can be controlled by varying the CVD process parameters. The unique lamellar, fine‐grained microstructures of these coatings contribute to their good tribological properties.

References

3