Journal of the American Ceramic Society · 2014 · 135 citations · 34 references
Natural SciencesMaterials EngineeringMaterials ScienceBiomaterialsCeramic MaterialsCeramicsBioactive GlassesBioceramicsCeramic BiomaterialsGlass MaterialsImplant MaterialsPorous CeramicsBioactive CeramicsBioactive Glass-ceramicsBioactivityBioactivity In Vitro TestingBioactivity TestingCeramic CharacterizationSol - Gel TransitionTemperature Effects
The study examined how aging time and temperature affect the structure and in vitro bioactivity of 45S5 glass‑ceramics. Porous 45S5 glass‑ceramics were fabricated via an acid‑catalyzed sol–gel process, characterized by FTIR to track hydroxyapatite formation in simulated body fluid, and their bioactivity was compared to that of amorphous Bioglass®. Higher aging time and temperature increased crystallization but reduced bioactivity over time; gel‑derived glass‑ceramics aged 3 days at 60 °C formed hydroxyapatite faster than amorphous Bioglass® within 7 days, and after 14 days both had comparable HA amounts, indicating that suitable aging can produce glass‑ceramics with bioactivity similar to amorphous Bioglass®.
Porous bioactive glass‐ceramics based on the 45S5 Bioglass ® composition were fabricated by an acid‐catalyzed sol–gel method. The effects of aging time and temperature on the structure and in vitro bioactivity were investigated. Fourier‐transform infrared spectroscopy ( FTIR ) was carried out on the samples to understand the structure and to monitor the formation of hydroxyapatite ( HA ) after immersion in simulated body fluid ( SBF ). The bioactivity of gel‐derived 45S5 glass‐ceramic and amorphous 45S5 Bioglass ® was compared. The results showed that an increase in both aging time and temperature can enhance crystallization, whereas bioactivity is reduced with increasing aging time but not significantly influenced by aging temperature. Compared with amorphous 45S5 Bioglass ® , gel‐derived glass‐ceramic aged for 3 d at 60°C exhibited a more rapid rate of HA formation after immersion for less than 7 d. Amorphous 45S5 Bioglass ® showed higher HA formation rate after immersion in SBF for more than 7 d, whereas the quantity of formed HA on gel‐derived 45S5 glass‐ceramic was still comparable to that of amorphous 45S5 Bioglass ® after immersion for 14 d. It is suggested that the lower bioactivity of 45S5 glass‐ceramics could be outweighed by the higher surface area and higher content of Si – NBO groups in gel‐derived glass‐ceramics. The results thus confirm that gel‐derived 45S5 glass‐ceramic exhibiting bioactivity comparable to that of amorphous 45S5 Bioglass ® can be fabricated by sol–gel method under suitable aging conditions.
34