IEEE Transactions on Magnetics · 1993 · 12 citations · 4 references
Natural SciencesMaterials EngineeringMaterials ScienceCeramic MaterialsMagnetic MaterialsThin FilmsAmorphous Magnetic MaterialsFerrimagnetic MaterialsMagnetic Properties Of SolidsMagnetic Thin FilmsMagnetization ProcessesThin Film Magnetic PropertiesFerrimagnetic Thin FilmsFerrite Thin FilmsFerritesHysteresis LoopsMagnetic PropertiesSputteringTemperature-dependent MagnetizationTorque
Strontium ferrite films were deposited by RF sputtering of a commercial strontium ferrite target onto fused quartz substrates maintained at temperatures up to 900 degrees C. Films deposited at T<800 degrees C were amorphous, but films deposited at T>800 degrees C had crystalline M-type strontium ferrite structures. The thin composition corresponded to that of the target. Films deposited at 800 degrees C were partially oriented in the [110] direction with the c-axis in the plane. Postannealing led to an increase in the magnetization, indicating incomplete formation of ferrite in the as-deposited state. Both in-plane and perpendicular hysteresis loops are rectangular with remanence ratios of 0.8 and 0.6, respectively, showing partial orientation with the c-axis. The torque curve is consistent with the above, although there are some additional anomalous peaks.< <ETX xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">></ETX>
4