Operative Dentistry · 2007 · 136 citations · 26 references
DentistryMaterials ScienceRestorative DentistryAgingOptical MaterialsAging EffectsAging TechniquesColor PreservationColor StabilityComposite Resin RestorationsDirect Composite RestorationsAging Color StabilityAging Effects On Material ColorAging Of Restorative MaterialsColor Appearance ChangesColor Stability After RestorationColor Stability AssessmentComposite Restorative MaterialsDirect Composite Bonding
PURPOSE: This study evaluated the color changes and amount of remaining C = C bonds (%RDB) in three dental composites after hydrothermal- and photoaging. METHODS AND MATERIALS: The materials tested were Estelite sigma, Filtek Supreme and Tetric Ceram. Specimens were fabricated from each material and subjected to L* a* b* colorimetry and FTIR spectroscopy before and after aging. Statistical evaluation of the deltaL,* deltaa,* deltab,* deltaE and %deltaRDB data was performed by one-way ANOVA and Tukey's test. The %RDB data before and after aging were statistically analyzed using two-way ANOVA and Student-Newman-Keuls test. In all cases an alpha = 0.05 significance level was used. RESULTS: No statistically significant differences were found in deltaL*, deltaa*, deltaE and %deltaRDB among the materials tested. Tetric Ceram demonstrated a significant difference in deltab*. All the materials showed visually perceptible (deltaE >1) but clinically acceptable values (deltaE < 3.3). Within each material group, statistically significant differences in %RDB were noticed before and after aging (p < 0.05). Filtek Supreme presented the lowest %RDB before aging, with Tetric Ceram presenting the lowest %RDB after aging (p < 0.05). The %deltaRDB mean values were statistically significantly different among all the groups tested. No correlation was found between deltaE and %deltaRDB.
26