Journal of the American Ceramic Society · 1997 · 51 citations · 46 references
Natural SciencesMaterials EngineeringMaterials ScienceCeramic MaterialsCeramicsMaterials ChemistryAluminum OxidesMetal OxidesPowder ProcessingStructural CeramicsCeramic SynthesisHexagonal LatticesHexagonal SystemMillingOxidationSilica-based Materials
An intimate Ba‐Al‐Al 2 O 3 ‐SiO 2 powder mixture, produced by high‐energy milling, was pressed to 3 mm thick cylinders (10 mm diameter) and hexagonal plates (6 mm edge‐to‐edge width). Heat treatments conducted from 300° to 1650°C in pure oxygen or air were used to transform these solid‐metal/oxide precursors into BaAl 2 Si 2 O 8 . Barium oxidation was completed, and a binary silicate compound, Ba 2 SiO 4 , had formed within 24 h at 300°C. After 72 h at 650°C, aluminum oxidation was completed, and an appreciable amount of BaAl 2 O 4 had formed. Diffraction peaks consistent with hexagonal BaAl 2 Si 2 O 8 , BaAl 2 O 4 , β‐BaSiO 3 , and possibly β‐BaSi 2 O 5 were detected after 24 h at 900°C. Diffraction peaks for BaAl 2 O 4 and BaAl 2 Si 2 O 8 were observed after 35 h at 1200°C, although SEM analyses also revealed fine silicate particles. Further reaction of this silicate with BaAl 2 O 4 at 1350° to 1650°C yielded a mixture of hexagonal and monoclinic BaAl 2 Si 2 O 8 . The observed reaction path was compared to prior work with other inorganic precursors to BaAl 2 Si 2 O 8 .
46
Oxidation of metals and alloys
Herbert H. Uhlig · Journal of Chemical Education · 1954 · 732 citations
Oxidation of Metals at High Temperatures
Walter J. Moore · Journal of The Electrochemical Society · 1953 · 378 citations