Natural SciencesMaterials EngineeringMaterials SciencePolymer ChemistryPolymer EngineeringPolymer MaterialsCrystalline MaterialsPolymer CharacterizationPolymer CrystallinityPolymer CrystallizationPolymer ExtrusionPolymer Thin FilmsCrystallization BehaviorCrystallization During ProcessingCrystallization MechanismsExtrusionMelting TemperaturePoly(lactic Acid)Tensile DeformationTensile Deformation Of Polymers
Abstract Melt‐crystallized films of poly( L ‐lactic acid) (PLLA) with M v in the range of 3.8 ∼ 46 × 10 4 consisting of α‐form crystals were uniaxially drawn by solid‐state coextrusion. The effects of M v , extrusion draw ratio (EDR), and extrusion temperature ( T ext ) on the crystal/crystal transformation from α‐ to β‐form crystals and the resultant tensile properties of drawn products were studied. The crystal transformation proceeded with EDR and more rapidly for the higher M v 's. Furthermore, the crystal transformation proceeded most rapidly with EDR at a T ext around 130 °C, independently of the M v 's. As a result of the optimum combination of processing variables influencing the the crystal transformation ( M v , T ext , and drawability), highly oriented films consisting of β‐form crystals alone were obtained by coextrusion of higher M v samples at T ext 's slightly below the melting temperature (150 ∼ 170 °C) and at higher EDR's > 11. Both the tensile modulus and strength increased rapidly with EDR. The modulus at a given EDR was slightly higher for the samples with higher M v 's. In contrast, the strength at a given EDR was remarkably higher for the higher M v 's. The highest tensile modulus of 8.0 GPa and strength of 500 MPa were obtained with the sample of the highest M v of 46 × 10 4 coextruded at 170 °C to the highest EDR of 14.
25
Molecular conformation of poly(S‐lactic acid)
P. De Santis, A. J. Kovacs · Biopolymers · 1968 · 565 citations