Natural SciencesChemistryMaterials ScienceInorganic ChemistryMaterials ChemistryPhase TransformationsCrystal LatticeCrystallization ProcessesInorganic MaterialsMetal OxidesSolid-state SynthesisTransition Metal ChemistryAmorphous OxidesCeramic SynthesisCubic Unit CellsHydrolysisRutile OxidesThermochemistry Of OxidesTitanium OxidesZinc Oxides
A compound tentatively denoted as Zn 2 Ti, 3 O 8 is determined to be a low‐temperature form of ZnTiO 3 . At a heating rate of 10°C·min −1 the low‐temperature form crystallizes at 600° to 765° C from an amorphous material prepared by the simultaneous hydrolysis of zinc acetylacetonate and titanium isopropoxide. It has a cubic unit cell with a =0.8408 nm. The cubic‐to‐hexagonal transformation occurs slowly above 820°C; during transformation ZnTiO 3 decomposes into Zn 2 TiO 4 and TiO 2 (rutile) at 965° to 1010°C. A single phase of the hexagonal form can be prepared by heating for 5 h at 900°C. The structure of both forms consists of octahedral TiO 6 groups.
7