A Correlation of Material Toughness, Thermal Shock Resistance, and Microstructure of High Tungsten, Silver-Tungsten Composite Materials

G. Witter, W. R. Warke

IEEE Transactions on Parts Hybrids and Packaging · 1975 · 17 citations · 3 references

Concepts

Abstract

The electrical erosion resistance of composite silver-tungsten materials seems to improve with finer dispersions of the silver and tungsten; however, these materials with the finer dispersions exhibit a higher tendency to fail by catastrophic crack propagation during arc erosion testing. A fracture mechanics approach is taken to determine G <inf xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">f</inf> c, the critical strain .energy release rate for crack extension under plane strain conditions for several compositions and particle size distributions of silver-tungsten materials. A qualitative analysis of resistance to crack propagation in the same materials under severe arcing agrees with the G <inf xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">l</inf> c measurements. The fracture toughness of these materials has also been compared to the microstructure by quantitative metallography. A relationship of G <inf xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">l</inf> <inf xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">c</inf> and the mean free path between tungsten particles has been found to agree on only a porton of the materials. A more complex term involving contiguity, volume fraction silver and mean free path has a good correlation with G <inf xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">l</inf> c for all the materials.

References

3