Temperature‐Dependent Iron Solubility in Mullite

Hartmut Scheider

Journal of the American Ceramic Society · 1987 · 19 citations · 4 references

Concepts

Abstract

Sample disks prepared from Al 2 O 3 (61 wt%), SiO 2 (28 wt%), and Fe 2 O 3 (II wt%) powders were sintered at 1270° and 1440°C and then annealed between 1300° and 1670°C. The annealed samples consisted of mullite as the main compound with minor amounts of glass and sometimes magnetite. The iron content of the mullites decreases strongly from ∼ 10.5 wt% Fe 2 O 3 at 1300°C to ∼ 2.5 wt% Fe 2 O 3 at 1670°C. A complex temperature‐controlled exsolution mechanism of iron from mullite is considered.

References

4