CORROSION · 1996 · 53 citations · 0 references
Natural SciencesMaterials EngineeringMaterials ScienceCorrosion ScienceMetallic MaterialsMetallurgyAlloysCorrosion EngineeringCorrosion MechanismsCorrosion ResistanceCorrosion-resistant MaterialsMetalsAmorphous AlloysAmorphous MetalsCorrosion BehaviorCorrosion Of Ferrous AlloysCorrosion Resistance MaterialsCorrosion-resistance MechanismsCorrosion-resistant AlloysNickel-based Alloys
The corrosion behavior of electrodeposited Ni-P, Ni-W, Ni-W-P, and Fe-W alloys was tested, and the effects of the additive elements W and P on the corrosion resistance of amorphous deposits were studied. Corroson rates of the alloys were compared to those of stainless steel. Results showed the W content in electrodeposited Ni-W-P amorphous alloy was as high as 55.2 wt%. The hardness (Vickers [HV]) of the alloy was from 700 HV to 800 HV and 1,300 HV to 1,400 HV after heat treatment at 550°C. The hardness, wear resistance, and corrosion resistance of the deposit were shown to be superior to those of Ni-P amorphous deposit.1 The corrosion potential (Ecorr) was moved to noble by adding P to the deposit, and the passive current density (ipass) dropped remarkably with the addition of W. Amorphous Ni-W, Ni-W-P, and Fe-W alloy deposits showed high corrosion resistance in acid solutions. Immersion tests in 1 mol/L (4.54 mol/gal) hydrochloric acid (HCl) solution at 30°C showed the corrosion rate of type 304 stainless steel (UNS S30400) was 10 times that of Ni-W-P amorphous deposit, 40 times that of Ni-W amorphous de-posit, and 15 to 20 times that of Fe-W amorphous deposit. In 0.5 mol/L (2.27 mol/gal) sulfuric acid (H2SO4) solution at 30°C, the corrosion resistance of the amorphous deposit was poorer than that of type 304 SS, but at 60°C, the corrosion rate of type 304 SS increased dramatically, to ~ 180 times that of Fe-W amorphous deposit and 100 to 700 times that of the Ni-based amorphous deposit.