Scintillation Properties of Praseodymium Doped LuAG Scintillator Compared to Cerium Doped LuAG, LSO and ${\rm LaBr} _{3}$

M. Moszyński, A. Nassalski, A. Syntfeld-Każuch, T. Szczęśniak, Kei Kamada, Kousuke Tsutsumi, Y. Usuki, Takayuki Yanagida, Akira Yoshikawa, Weerapong Chewpraditkul,

IEEE Transactions on Nuclear Science · 2009 · 59 citations · 26 references

Concepts

Abstract

Properties of praseodymium and cerium doped Lutetium Aluminum Garnet (LuAG) were compared with cerium doped Lutetium Oxyorthosilicate (LSO) and Lanthanum Bromide (LaBr <sub xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">3</sub> ). Light yield, its non-proportionality relative to 662 keV gamma -rays and the dependence of the energy resolution on energy of the detected gamma -rays were measured. LuAG:Pr turned out to have good proportionality, with deviation from unity around 10% at 16.6 keV and 3% at 59.5 keV. This, together with relatively high light yield of 5600 phe/MeV results in a very good energy resolution of LuAG:Pr of 5.1% measured with 662 keV gamma-rays. The measured time resolution of 308 ps is significantly larger than that of 166 ps obtained for LSO:Ce. This can be explained by smaller light yield of LuAG:Pr and the fact that only about 25% of its scintillation is emitted in short decay time modes of 17.6 ns and 52 ns, while the rest is decaying with long time modes of 1.4 mus and 9 mus.

References

26