Lithium Insertion/Deinsertion Characteristics of Nanostructured Amorphous Tantalum Oxide Thin Films

Hoang X. Dang, Yong‐Mao Lin, Kyle C. Klavetter, Trevor H. Cell, Adam Heller, C. Buddie Mullins

ChemElectroChem · 2013 · 34 citations · 37 references

Concepts

Abstract

Abstract Lithium uptake and release by pure, morphology‐controlled Ta 2 O 5 films is studied. Porous nanocolumnar films, reactively e‐beam deposited at 70° versus normal, are rapidly lithiated and delithiated, withstanding volume‐change‐associated stresses. Their reversible gravimetric Coulombic capacities at 1 C, 2 C, 5 C, and 10 C rates are, respectively, 252, 225, 192, 168 mAh g −1 . After 100 cycles at 1 C rate the films retain 96 % of their Coulombic capacity and 99 % of their Coulombic efficiency. The rapid lithiation/delithiation is attributed to formation of amorphous, Li + permeable, nanoporous LiTaO 3 .

References

37