CORROSION · 1993 · 66 citations · 10 references
Natural SciencesMaterials EngineeringMaterials ScienceMechanical Behavior Of MaterialsMetallic MaterialsMetallurgyAlloysCorrosion Of SteelsFracture MechanicsFracture ToughnessMetalsSteel MaterialsAlloying ElementsHigh Strength Low Alloy SteelsHigh-strength Steel AlloysHydrogen Embrittlement Of SteelsHydrogen-induced CrackingSynergistic ImpactsTransformation Products
The effects of alloying elements such as niobium, copper, chromium, molybdenum, and titanium in high-strength, low-alloy (HSLA) steels on hydrogen induced cracking (HIC) were investigated. The HIC test was performed to NACE TM-02-84 in BP (saturated H2S synthetic sea water) and NACE solutions. The test data were analyzed with an optical microscope, scanning electron microscope, electron probe microanalyzer, Auger electron spectrometer, transmission electron microscope, and an image analyzer. Results showed the addition of Nb increased the aspect ratio of inclusions and decreased HIC resistance. In BP solution, Cu-bearing steel formed a protective film of γ-Fe2O3 enriched with Cu on the outside and FeS on the inside. Cr and Mo showed a synergistic effect on the formation of low-temperature transformation products and the increase of HIC sensitivity. The suitable parameter for these two elements on HIC sensitivity was Cr15+Mo5, and the critical value of this parameter was 0.1%. Additionally, coarse TiN precipitates, as well as elongated MnS inclusions, were the initiation sites of HIC. Both cooperated to result in HIC.
10
Hiroshi Tamehiro, Tetsuo Takeda, Shôichi Matsuda et al. · Transactions of the Iron and Steel Institute of Japan · 1985 · 67 citations · Full text