PZT 52/48 Depolarization: Quasi-Static Thermal Heating Versus Longitudinal Explosive Shock

Sergey I. Shkuratov, Jason Baird, Vladimir G. Antipov, E. F. Talantsev, Christopher S. Lynch, Larry L. Altgilbers

IEEE Transactions on Plasma Science · 2010 · 21 citations · 25 references

Concepts

Abstract

Systematic studies of the depolarization of Pb(Zr <sub xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">0.52</sub> Ti <sub xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">0.48</sub> )O <sub xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">3</sub> (PZT 52/48) poled piezoelectric ceramic samples were performed using thermal heating and explosive longitudinal-shock compression. The electric charge density that is released due to thermal heating at a rate of 0.9 K/min was consistent for all sample sizes (Q = 27.8 μC/cm <sup xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">2</sup> ). The charge density that is released due to shock compression was practically equal to that released due to thermal heating. The PZT 52/48 samples were completely depolarized by longitudinal shock waves at shock front pressures of P <sub xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">SW</sub> = 1.5 ±0.2 GPa. The electric charge that the samples release can be transformed into pulsed power. Miniature explosive-driven ferroelectric generators containing PZT 52/48 ceramic elements with a volume of 0.35-3.5 cm <sup xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">3</sup> are capable of converting the depolarization charge into pulses of high voltage with amplitudes of up to 22 kV and high power with a peak power of up to 0.35 MW within a time interval of 0.3-1.5 μs .

References

25