The Angle Orthodontist · 2014 · 16 citations · 17 references
DentistryMaterials EngineeringMechanical Behavior Of MaterialsMechanical Properties Of Dental MaterialsSurface Properties Of Dental MaterialsDenture Base MaterialsMaterials For Maxillofacial ProsthesesArchwire Material PropertiesCoating HardnessElastic Modulus MeasurementFourier Transform Infrared SpectroscopyMaterial Composition AnalysisOrthodontic ArchwiresOrthodontic Material TestingScratch Test Parameters
OBJECTIVE: To evaluate the material composition, mechanical properties (hardness and elastic modulus), and scratch resistance of the coating of four commercialized esthetic orthodontic archwires. MATERIALS AND METHODS: The coating composition of esthetic archwires was assessed by Fourier-transform infrared spectroscopy (FTIR). Coating hardness and elastic modulus were analyzed with instrumented nano-indentation tests. Scratch resistance of coatings was evaluated by scratch test. Coating micromorphologic characteristics after scratch tests were observed in a scanning electron microscope. Statistical differences were investigated using analysis of variance and Tukey post hoc test. RESULTS: The FTIR results indicate that all analyzed coatings were markedly characterized by the benzene peak at about 1500 cm(-1). The coating hardness and elastic modulus average values ranged from 0.17 to 0.23 GPa and from 5.0 to 7.6 GPa, respectively. Scratch test showed a high coating elasticity after load removal with elastic recoveries >60%, but different failure features could be observed along the scratches. CONCLUSION: The coatings of esthetic archwires evaluated are probably a composite of polyester and polytetrafluoroethylene. Delamination, crack propagation, and debris generation could be observed along the coating scratches and could influence its durability in the oral environment.
17