ECS Journal of Solid State Science and Technology · 2013 · 24 citations · 26 references
Natural SciencesMaterials EngineeringMaterials ScienceMaterials ChemistryOptical MaterialsThin FilmsIron OxidesOptical Thin FilmsThin Film Optical PropertiesThin-film DepositionThin-film MaterialsCrystallite Size AnalysisMetallic Thin FilmsOptical AbsorptionThermal Treatment
We report on a method to deposit iron pyrite thin films via chemical bath deposition of Fe-O-S thin films followed by their thermal treatment in a sulfur-rich ambient. The deposition is made on glass substrates from an aqueous solution mixture of iron(III) nitrate, sodium thiosulfate, triethanolamine, and HCl added to adjust the pH between 7–8. After 2.5 h of deposition at 40°C, a uniform specularly reflective amorphous film with thickness of 315 nm is obtained with a S:Fe ratio of 0.44 and significant oxygen content. Optical bandgap (Eg) of this material is 2.56 eV. Upon heating this film in a N2/S ambient at 400°C for 3–10 h, a dark-gray mirror-like film is obtained. The film attains a granular morphology and the S:Fe ratio approximates to 2. This thin film is polycrystalline with cubic structure, as that of FeS2-pyrite phase, with crystallite diameter of 15 nm. Orthorhombic FeS2-marcasite is present as a minor phase in the film. The film possesses optical absorption coefficient 2 × 105 cm−1 in the visible region; indirect Eg of 0.85 eV; p-type electrical conductivity of 1.2–2.1 Ω−1 cm−1 showing photoconductivity; carrier density, 3 × 1017 cm−3; and Hall mobility, 14 cm2 V−1 s−1.
26