Surface and Interface Analysis · 1988 · 63 citations · 12 references
Natural SciencesMaterials EngineeringMaterials ScienceMaterials ChemistryMetallurgyPhase TransformationsAlloysAluminum OxidesGrain GrowthKinetics Of Phase TransformationsMicrostructure EvolutionOxidation ReactionsAluminaAluminium AlloysGrain BoundariesOxide Scale FormationOxide Scale GrowthOxygen Transport KineticsScale Growth MechanismsTransition Metal Oxides
Abstract Small additions of yttrium to NiAl result in a decreasing oxygen transport through the Al 2 O 3 scale on AiAl at 1270 K, as has been shown by nuclear reaction analysis ( 18 O(p, α) 15 N). A higher concentration, e.g. 0.5 wt%, has the opposite effect. Yttrium segregates to the grain boundaries in the alloy, and an enhanced Y concentration has been observed by means of EPMA in the oxide scale above the grain boundaries of the alloy. Transition aluminium oxides are shown to be formed in the initial stage at 1170 K with (glancing angle) x‐ray diffraction. Only α‐Al 2 O 3 is formed after oxidation for several minutes at higher temperatures (1470 K). The rate of transformation of transition Al 2 O 3 to the stable α‐Al 2 O 3 modification depends on the oxidation temperature. The transition is shown to be retarded by the presence of Y. The primary transport processes in the Al 2 O 3 scales are short‐circuit diffusion of oxygen and/or aluminium. At 1170 K, while transition oxides are still present, Al transport predominates. At higher temperatures, when the oxide has the α‐Al 2 O 3 structure, oxygen transport is enhanced. This would also explain the retardation of oxygen transport by the addition of Y, since Y was found to prevent the formation of the most stable form of Al 2 O 3 .
12