Chemical Communications · 2012 · 42 citations · 38 references
The simultaneous improvement of the melting temperature (T(m) = 224 °C) and the decomposition temperature (T(10) = 359 °C) of poly(lactide)s was achieved by the stereocomplex formation of poly(l-lactide) and poly(d-lactide) with bio-based aromatic groups at both initiating and terminating chain ends.
38
Chitin and chitosan: Properties and applications
Marguerite Rinaudo · Progress in Polymer Science · 2006 · 7.8K citations
Stereocomplex formation between enantiomeric poly(lactides)
Hideto Tsuji · Macromolecules · 1987 · 1.4K citations