OSTI OAI (U.S. Department of Energy Office of Scientific and Technical Information) · 1983 · 19 citations · 0 references
ArchitectureMaterials ScienceAtmospheric RadiationBuilding MaterialsWood ConservationOutdoor Light ExposureWood DecayWood DeteriorationWood MaterialsColor In Wood MaterialsFree Radical GenerationMoisture-damage InteractionPhoto-damageRadiation-induced Free RadicalsSinglet Oxygen GenerationUltraviolet Light ExposureWood Surface Properties
Wood materials are sensitive to outdoor weathering. The major significant factors causing weathering, such as solar radiation (ultraviolet light), moisture, and oxygen, have been investigated. It was found that UV light cannot penetrate deeper than 75 ..mu..m, while visible light can penetrate 200 ..mu..m into wood surfaces. Loss of brightness and change of color occurred when wood was exposed outdoors. SEM micrographs showed that most of the cell walls on exposed transverse surfaces were separated at the middle lamella region after 500 h of UV irradiation. Half-bordered and bordered pits on exposed radial surfaces were severely damaged by light. Free radicals were generated at the wood surface during irradiation. The rate of free radical formation was enhanced when the moisture content in wood increased from zero to 6.3%, but beyond this stage the rate of radical decay increased. ESR and UV studies on the behavior of free radicals generated and their interaction with oxygen molecules to form hydroperoxides revealed that free radicals and singlet oxygen played important roles in discoloration and deterioration reactions. IR studies showed that carbonyl and carboxylic groups were formed in cellulose and lignin on the exposed wood surfaces. The lignin content was reduced with increasing irradiationmore » time. The photo-oxidative effect can be mitigated by treating wood surfaces with an aqueous solution of chromic acid and ferric chloride. Only relatively small amounts of these chemicals are needed for effective protection. Possible chemistry and mechanisms of degradation and protection are discussed. 31 references, 18 figures, 2 tables.« less