Journal of the American Ceramic Society · 2000 · 77 citations · 18 references
Natural SciencesMaterials EngineeringMaterials ScienceCeramic MaterialsCeramicsMaterials ChemistryDielectric CeramicsElectrical Properties Of CeramicsPorous CeramicsPowder ProcessingSinteringStructural CeramicsBarium Titanate CeramicsElectrical CeramicsLead Zirconate TitanateLead Zirconate Titanate CeramicsPermittivityPowder CharacterizationSintering BehaviorSpark Plasma Sintering
Dense PbTiO 3 ceramics consisting of submicrometer‐sized grains were prepared using the spark‐plasma‐sintering (SPS) method. Hydrothermally prepared PbTiO 3 (0.1 μm) was used as a starting powder. The powder was densified to ≳98% of the theoretical X‐ray density by the SPS process. The average grain size of the spark‐plasma‐sintered ceramics (SPS ceramics) was ≲1 μm, even after sintering at 900°–1100°C, because of the short sintering period (1–3 min). The measured permittivity of the SPS ceramics showed almost no frequency dependence over the range 10 1 –10 6 Hz, mainly because pores were absent from the ceramics. The coercive field of the SPS ceramics was somewhat higher than that of conventionally sintered ceramics, which could be attributed to the small‐grained microstructures of the SPS ceramics.
18
Masao Tokita · Journal of the Society of Powder Technology Japan · 1993 · 610 citations · Full text
On the Phase Transition in Lead Titanate
G. Shirane, Sadao Hoshino · Journal of the Physical Society of Japan · 1951 · 394 citations