Toughening of Epoxy Resins with Thermoplastics: 3. An Investigation into the Effects of Composition on the Properties of Epoxy Resin Blends

D. J. Hourston, J. Lane, H. X. Zhang

Polymer International · 1997 · 81 citations · 0 references

Concepts

TL;DR

The study compared the toughenabilities of various epoxy resin mixtures. Blends of three epoxy resins (DGEBA, TGPAP, TGDDM) were mixed in varying proportions, cured with two curing agents, and their dynamic mechanical and fracture properties were measured, with additional PEI added in varying amounts to toughen the resins. The blends cured homogeneously; glass transition temperature varied systematically with composition, while G1c and K1c varied little; the 75/25 TGPAP/DGEBA mixture was the most toughenable, and adding 20 % PEI more than tripled the G1c value. © SCI.

Abstract

Three different epoxy resins, based on the diglycidylether of bisphenol A (DGEBA), triglycidyl-p-aminophenol (TGPAP) and tetra-glycidyldiaminodiphenylmethane (TGDDM), which are di-, tri- and tetrafunctional, respectively, were mixed in varying proportions and cured with both 3,3′-diaminodiphenylsulphone and 4,4′-[1,4-phenylene(1-methylethylidene)]bis(2,6-dimethylbenzenamine) (EPON 1062-M from Shell). All the blends could be satisfactorily cured and gave homogeneous materials. The dynamic mechanical and fracture properties of the cured materials were measured. It was found that the glass transition temperature varied with composition systematically, whereas values of the strain energy release rate (G1c) and the stress intensity factor (K1c) showed relatively small variations with the blend composition. Toughened epoxy resins were prepared by adding a polyetherimide (PEI), in varying proportions, to the resin mixture. The 'toughenabilities' of different resins, or resin mixtures, were compared. This showed that the 75/25 TGPAP/DGEBA resin mixture was the most toughenable. Adding 20% of PEI led to a more than three-fold increase of the G1c value. © of SCI.