Microstructure, Strength, and Oxidation of a 10 wt% Zyttrite‐Si <sub>3</sub> N <sub>4</sub> Ceramic

Sunil Dutta, B. C. Buzek

Journal of the American Ceramic Society · 1984 · 40 citations · 7 references

Concepts

Abstract

Hot‐pressed Si 3 N 4 doped with 10 wt% zvttrite as a sinterine aid was studied. An equiaxed, fine‐grainid microstructure was predominant, with no apparent porosity. Bend strengths were determined at room temperature and high temperatures (up to 1370°C/2500°F). Oxidation was measured by weight gain at 1370°C in air. The resulting material exhibited very good room‐temperature strength (755 MPa/110 ksi). The work showed that room‐temperature strength can be improved significantly by using controlled Si 3 N 4 powder with 10 wt% zyttrite. High‐temperature strength (514 MPd75 ksi) at 1370°C was nearly double that of hot‐pressed Si 3 N 4 (NC‐132). The oxidation resistance at 1370°C was also higher than that of NC‐132.