Journal of Biomedical Materials Research · 1968 · 22 citations · 9 references
Natural SciencesDental Biomaterials ScienceDental Materials ScienceDental MaterialsElectroanalytical MethodsElectrochemistryDental AmalgamElectroanalytical ChemistryElectrochemical KineticsElectrode KineticsElectrode MaterialsElectrode PotentialsAmalgam Alloy CompositionAmalgam CompositionAnodic PolarizationElectrochemical BehaviorElectrochemical CharacterizationElectrochemical PotentialsPolarizationStandard Hydrogen Electrode
Abstract The effects of variations in composition and processing on the open‐circuit electrode potentials measured as a function of time of amalgams made from silver–tin, silver–tin–copper, silver–tin–zinc, and silver–tin–copper–zinc alloys have been determined at 37°C in distilled water, in saline solution, as well as in acetate and citrate solutions buffered to pH values of 3, 7, and 10. The electrochemical potentials of the alloys measured as a function of time in neutral acetate solutions show anodic polarization from an initial cathodic potential value of approximately 0.1 v with respect to the standard hydrogen electrode to a constant potential level depending upon alloy composition. In neutral acetate solution the potential–time curves of silver–tin amalgams with 7:5 mercury to alloy ratio show a rapid anodic polarization from an initial anodic potential value of 0.28 v to a minimum value of 0.05 v at approximately 1 hr followed by a potential reversal to a plateau value of 0.40 v. For 7:5 amalgams in neutral acetate solutions increases in both the trituration time and in the severity of processing deformation cause a small increase in initial potential, with a decrease in anodic polarization, while an increase in amalgam age lowers both the initial potential value and the longer‐time potential plateau. Increasing the mercury content of the amalgam to a 2:1 ratio decreases the rate of potential reversal from the minimum, whereas decreasing the ratio to 4:5 decreases the amount of depolarization from the minimum value. The effects of copper and zinc additions to silver–tin alloys are mixed. In neutral acetate solution the 7:5 ratio amalgams from silver–tin–copper alloys show anodic polarization from the same initial value as the silver–tin amalgams, followed by a region of decreased polarization. Both silver–tin–zinc and silver–tin–copper–zinc alloys exhibit a much higher initial anodic potential (0.78 v), and following the achievement of the potential plateau have a slow anodic polarization to the long‐time potential value shown by silver–tin amalgam. Three commercial alloy amalgams were studied in neutral acetate solution. The two amalgams containing zinc have a potential behavior similar to that of the experimental zinc‐containing amalgam; the non‐zinc amalgam shows a rapid anodic polarization from an initial anodic potential value of 0.24 v, a minimum at 1 hr, and a reversal to the long‐time potential values of 0.40 v shown by the zinc‐containing amalgam.
9