Journal of Polymer Science Polymer Chemistry Edition · 1977 · 93 citations · 14 references
Natural SciencesChemistryMaterials ScienceMaterials ChemistryPolymer ChemistryPolymer MaterialsPolymer CharacterizationPolymer Physical ChemistryPolymer PhysicsPolymer ProcessingPolymer Thin FilmsPolymerization ChemistryInfrared Absorption SpectraInfrared SpectraLight ScatteringLight Scattering AnalysisMelting TemperatureMelting Temperature AnalysisPolyamidePolymer Molecular Characteristics
Abstract Nylon 46 was synthesized from the salt of 1,4‐diaminobutane and adipic acid. High molecular weight polymers could be obtained by reaction for 1 hr at 215°C in a closed system and at least for 1 hr in vacuo at a temperature in the range 290–305°C. The reactions at 290°C were found to have taken place in the solid state and those at 305°C in the melt. The highest molecular weights ( M̄ w ca. 45,000) were obtained by reaction at 290°C with a nylon salt with a pH of 7.8–8.0. The molecular weight characteristics were studied with end‐group analysis, viscometry, light scattering, and ultracentrifugation. The polymers were found to be gel‐free and monodisperse ( M̄ w / M̄ n ∼ 1.15). Films could be cast from formic acid. From x‐ray diffraction patterns, measured on such films, spacings of 3.74 and 4.30 Å were calculated, whereas a long period of 66 Å was also found. The infrared spectra showed all the usual amide bands of even–even polyamides. The melting temperature was found to vary between 283 and 319°C, depending on the thermal history of the sample. Water absorption measured on a cast film showed this to be very hygroscopic (7.5% at 65% RH), while a highly crystalline sample absorbed only little water (1.6% at 65% RH).
14
Determination of Molecular Weight of Nylon
J. E. Waltz, G. B. Taylor · Analytical Chemistry · 1947 · 154 citations