Synthesis and characterization of poly(arylene ether sulfone) copolymers with sulfonimide side groups for a proton‐exchange membrane

53

Citations

22

References

2006

Year

Abstract

Abstract A sulfonimide‐containing comonomer derived from 4,4′‐dichlorodiphenylsulfone was synthesized and copolymerized with 4,4′‐dichlorodiphenylsulfone and 4,4′‐biphenol to prepare sulfonimide‐containing poly(arylene ether sulfone) random copolymers (BPSIs). These copolymers showed slightly higher water uptake than disulfonated poly(arylene ether sulfone) copolymer (BPSH) controls, but their proton‐conductivity values were very comparable to those of the BPSH series with similar ion contents. The proton conductivity increased with the temperature for both systems. For samples with 30 mol % ionic groups, BPSI showed less temperature dependence in proton conductivity and slightly higher methanol permeability in comparison with BPSH. The thermal characterization of the sulfonimide copolymers showed that both the acid and salt forms were stable up to 250 °C under a nitrogen atmosphere. The results suggested that the presumed enhanced stability of the sulfonimide systems did not translate into higher protonic conductivity in liquid water. © 2006 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 44: 6007–6014, 2006

References

YearCitations

Page 1