Effects of iron oxidation state on viscosity, lunar composition 15555

M. Cukierman, D. R. Uhlmann

Journal of Geophysical Research Atmospheres · 1974 · 52 citations · 7 references

Concepts

Abstract

The viscous flow behavior of lunar composition 15555, which contains about 22.5 wt % FeO, has been determined over a range of temperature from 620° to 700°C and from 1215° to 1400°C. The material was synthesized under mildly reducing conditions to simulate the Fe2+ /total Fe ratio of the lunar environment. The effect of iron oxidation state on flow behavior in the high-viscosity region has been evaluated for specimens of the 15555 composition having Fe2+/ total Fe ratios of 0.94, 0.76, and 0.20. Change of the Fe2+ concentration ratio from 0.94 to 0.76 had no observable effect on the viscosity; change of the ratio from 0.76 to 0.20 resulted in a dramatic increase in viscosity by some 3 orders of magnitude at a given temperature but did not change the form of the variation of viscosity with temperature. The flow behavior is discussed and related to the structural features of the glasses.

References

7