Journal of the American Ceramic Society · 1990 · 41 citations · 15 references
Natural SciencesChemistryMaterials ScienceColloid ScienceNanomaterialsPhysical ChemistryAluminum HydroxidesColloid ChemistryColloidal CrystallizationCrystallization ProcessesNanoparticle DispersionsNanoparticle SynthesisColloid CharacterizationColloidal NanoparticlesColloidal SolutionsColloidal SynthesisFibrous MaterialsHydrothermal SynthesisMetal Oxide Nanoparticle SynthesisMonodisperse Nanoparticle Synthesis
The synthesis of colloidal boehmite (AlOOH) is studied by heating basic aluminum chloride solutions under constant stirring. The temperature and Al 2 O 3 : Cl molar ratio influence the product morphology. Synthesis at 140°C generates highly fibrous polycrystalline particles that are on average 360 nm long, 30 nm broad, and 8 nm thick. They contain 0.11 mol of excess H 2 O per 1 mol of AlOOH. Synthesis at temperatures between 140° and 190°C produces broader fibrils and less excess H 2 O. Preparation at 220°C eventually produces fully crystalline platelike boehmite particles about 260 nm long, 95 nm broad, and 14 nm thick, without excess H 2 O. Fibril synthesis requires an Al 2 O 3 :Cl molar ratio exceeding 1.0 to yield noncoagulated particles. The fibrils are fairly monodisperse with 20% standard deviation in their length for an Al 2 O 3 : Cl molar ratio about 1.0.
15