Nano Letters · 2011 · 146 citations · 20 references
EngineeringMaterials EngineeringMaterials ScienceNanomaterialsNanotechnologyOptoelectronicsEtching ProcessesNanowiresSemiconductor Device MaterialsSemiconductor LasersSemiconductor NanomaterialsSemiconductor SurfacesDevice FabricationDry EtchingEtch RateEtchingSemiconductor Laser FabricationSemiconductor NanowiresWet Chemical EtchingWet Etching
Periodic high aspect ratio GaAs nanopillars with widths in the range of 500-1000 nm are produced by metal-assisted chemical etching (MacEtch) using n-type (100) GaAs substrates and Au catalyst films patterned with soft lithography. Depending on the etchant concentration and etching temperature, GaAs nanowires with either vertical or undulating sidewalls are formed with an etch rate of 1-2 μm/min. The realization of high aspect ratio III-V nanostructure arrays by wet etching can potentially transform the fabrication of a variety of optoelectronic device structures including distributed Bragg reflector (DBR) and distributed feedback (DFB) semiconductor lasers, where the surface grating is currently fabricated by dry etching.
20
Enhanced thermoelectric performance of rough silicon nanowires
Allon I. Hochbaum, Renkun Chen, Raul Diaz Delgado et al. · Nature · 2008 · 4.1K citations
Natural Sciences, Materials Engineering, Materials Science +14
Ruoxue Yan, Daniel J. Gargas, Peidong Yang · Nature Photonics · 2009 · 1.6K citations
Natural Sciences, Materials Engineering, Materials Science +17