Abstract Zintl phase compounds with large unit cells and complex anionic structures such as Yb 11 Sb 10 hold potential for being good thermoelectric materials. Single crystals of Ge‐doped Yb 11 Sb 10 were synthesized using a molten Sn‐flux technique. Single crystal X‐ray diffraction data were obtained and resulted in a composition of Yb 11 Sb 9.3 Ge 0.5 which was verified by microprobe. Yb 11 Sb 9.3 Ge 0.5 is isostructural to Ho 11 Ge 10 , crystallizing in a body‐centered, tetragonal unit cell, space group I 4/ mmm , with Z = 4. The unit cell parameters of Yb 11 Sb 9.3 Ge 0.5 are a = 11.8813(4), c = 17.1276(13) Å with a volume of 2417.8(2) Å 3 . These parameters correlate well with the structural refinement of previously published Yb 11 Sb 10 . The structure consists of 16 isolated Sb 3− anions, 8 $\rm Sb^{4-}_{2}$ dumbbells, 2 $\rm Sb^{4-}_{4}$ square planar rings and 44 Yb 2+ cations. The Ge, doped in at 28 % occupancy, was found to be site specific, residing on the 2 $\rm Sb^{4-}_{4}$ square planar rings. Single crystal X‐ray diffraction is most consistent with the site that makes up the square ring being less than fully occupied. The doped compound is additionally characterized by X‐ray powder diffraction, differential scanning calorimetry and thermogravimetry. High temperature (300–1200 K) thermoelectric properties show that the doped compound has extremely low thermal conductivity (10–30 mW/cmK), lower than that of Yb 11 Sb 10 . Temperature dependent resistivity is consistent with a heavily doped semiconductor. Yb 11 Sb 9.3 Ge 0.5 shows p‐type behavior increasing from ∼22 μV/K at room temperature to ∼31 μV/K at 1140 K. The low value and the temperature dependence of the Seebeck coefficient suggest that bipolar conduction produces a compensated Seebeck coefficient and consequently a low zT.

References

22