Synthesis, Densification, and Conductivity Characteristics of BICUVOX Oxygen‐Ion‐Conducting Ceramics

Steven P. Simner, D. Suarez‐Sandoval, John D. Mackenzie, Bruce Dunn

Journal of the American Ceramic Society · 1997 · 85 citations · 21 references

Concepts

Abstract

Copper‐substituted bismuth vanadate (Bi 2 V 0.9 Cu 0.1 O 5.35 ), known as BICUVOX, possesses high oxygen ion conductivities at low temperatures. The ionic conductivity of this material at 300°C (∼1 × 10 −3 S/cm) is 50 to 100 times greater than any other solid electrolyte in this temperature range. In this paper we report the preparation of sinterable BICUVOX powders by solid‐state reaction and conventional ceramic powder processing techniques. Densification studies indicate that optimum densities (>95% theoretical) can be obtained after 10‐20 h sintering at 800°C. Ionic conductivity characteristics were evaluated with respect to temperature, sample density, and prolonged isothermal heating.

References