Origin of porosity in titania gels. I. Microporous and mesoporous gels prepared from titanous chloride and ammonia

Jehane Ragaï, K. S. W. Sing, Raouf Sh. Mikhail

Journal of Chemical Technology and Biotechnology · 1980 · 30 citations · 11 references

Concepts

Abstract

Abstract Titania gels were prepared by oxidation of precipitates of hydrous Ti III oxide obtained at different pH values from aqueous titanous chloride by the addition of ammonia. The gels were dried at 110–120°C (383–393 K) and their surface properties were characterised by nitrogen adsorption at 196°C (77 K). The nitrogen isotherms have been analysed by the BET and α s ‐methods. Gels prepared at pH values of 3.30, 5.01, 6.20 and 7.10 were all mesoporous; the pore volume increasing with increase of pH, over the range studied. The gel prepared at pH 2.30 had a small micropore volume, whereas the gel prepared at pH 5.01 and aged for 6 months in water had a much larger micropore volume. The formation of the mesopore structure appears to be due to a condensation‐polymerisation process associated with the creation of hydroxo and oxo bridges between neighbouring Ti 3+ ions. If stabilising ligands (H 2 O or NH 3 ) are allowed to remain attached to the cations, the condensation‐polymerisation process is retarded and microporosity results.

References

11