Polymer-Plastics Technology and Engineering · 2005 · 23 citations · 9 references
Natural SciencesMaterials EngineeringMaterials SciencePolymer ChemistryPolymer EngineeringPolymer MaterialsComposite MaterialsThermoplastic PolymersButadiene RubberEthylene Propylene Diene Monomer RubberFatigue ResistanceMechanical Fatigue ResistanceRubber SwellingSwellingThermal StabilityVulcanization
Abstract: Butadiene-acrylonitrile rubber (NBR) was blended with ethylene- propylene-diene rubber (EPDM) in the presence and absence of different amounts of bromobutyl rubber (BIIR) to be tested as a compatibilizer. The results revealed that 10 phr was the optimum amount of BIIR to get a compatible blend. Dicumyl peroxide (DCP) curing system resulted in EPDM/NBR vulcanizates with better thermal aging resistance than did sulfur vulcanizates. Also DCP produced vulcanizates with the most reduced swelling values both in motor oil and brake fluid. On the other hand, sulfur-curing systems produced EPDM/NBR vulcanizates with much higher mechanical properties than did DCP vulcanizates. The fatigue resistance of the vulcanizates was greatly improved upon blending the two types of rubber. Also, the 25/75 EPDM/NBR blend possessed the highest aged mechanical properties together with good thermal stability. Keywords: NBREPDMepoxidized EPDMelastomer blendcompatibilizer Notes a MBT = mercapto benzothiazole. b CBS = N-cyclohexyl 2-benzothiazole sulphenamide. c HAF = high abrasion furnace black. d DCP = dicumylperoxide. a PAN = phenyl α-naphthyl amine.
9
Characterization of elastomer blend and compatibility
D. K. Setua, K. N. Pandey, A. K. Saxena et al. · Journal of Applied Polymer Science · 1999 · 38 citations
Natural Sciences, Materials Engineering, Materials Science +10
A. F. Younan, S. L. Abd‐El‐Messieh, Alain Gasser · Journal of Applied Polymer Science · 1998 · 32 citations
Natural Sciences, Materials Engineering, Materials Science +17