Natural SciencesMaterials EngineeringMaterials ScienceCeramic MaterialsCeramicsMaterials ChemistryCeramic ProcessingGrain GrowthThermodynamics Of CeramicsActivation EnergyDensificationDensification KineticsDensification MechanismsFerroelectric PropertiesGrain Boundary SlidingLead Zirconate TitanateLead Zirconate Titanate Ceramics
Grain growth and densification were studied in a hot‐pressed ferroelectric composition of 65/35 (Zr/Ti molar ratio) lead zirconate‐lead titanate containing 2 at.% bismuth. The grain growth and densification rate processes were measurable from 1050° to 1300°C and from 700° to 1100°C, respectively. Grain growth as a function of time followed a ⅓ power law ( D (grain size) = kt ⅓ ). An activation energy of 95 kcal/mole was calculated. Densification was a two‐stage process as a function of time: a rapid initial stage and a slower final stage. The initial stage of densification behaved viscously with an activation energy of 36.7 kcal/mole. Grain boundary sliding and the Nabarro‐Herring mechanism of stress‐directed movement of vacancies are suggested as the densification mechanisms. Results indicated that densification is sensitive to stoichiometry and to additives.
12
Diffusional Viscosity of a Polycrystalline Solid
Conyers Herring · Journal of Applied Physics · 1950 · 2.5K citations
Recrystallization and grain growth
Jan Burke, David Turnbull · Progress in Metal Physics · 1952 · 1.5K citations