Journal of the American Ceramic Society · 2000 · 75 citations · 15 references
EngineeringMaterials EngineeringMaterials ScienceCeramic MaterialsCeramicsMaterials ProcessingCeramic ProcessingComposite MaterialsFiber PropertiesSilicon MaterialsThermal Properties Of CeramicsThermogravimetric AnalysisFibersPolymer PyrolysisPyrolysis BehaviorSilicon Carbide (Sic) MaterialsSilicon Carbide CeramicsSilicon Carbide Composites
SiC‐based fibers with various chemical compositions were synthesized using an irradiation‐curing process. Polycarbosilane (PCS) fibers were cured by irradiation with an electron beam in a helium atmosphere. The cured PCS fibers were pyrolyzed at 1300°C under controlled hydrogen or argon atmospheres, and SiC fibers with C/Si of 0.84 to 1.56 were obtained. The fibers consisted of <1.0 wt% O, <0.2 wt% N, <0.1 wt% H, with the balance being Si and C. The mechanism of pyrolytic transformation of cured PCS to SiC‐based ceramics was investigated using TG/DTA analysis. Greater mass losses were observed during pyrolysis in a hydrogen atmosphere than in argon. This result suggests that the hydrogen atmosphere suppresses H 2 evolution and helps to remove excess carbon as CH 4 during pyrolysis. The microstructure and mechanical properties of the resulting SiC‐based fibers were found to be very dependent on their C/Si chemical compositions.
15
Development of a silicon carbide fibre with high tensile strength
Setsuko Yajima, J. Hayashi, Mika Omori et al. · Nature · 1976 · 554 citations
Natural Sciences, Materials Engineering, Materials Science +14
High-strength alkali-resistant sintered SiC fibre stable to 2,200 °C
Toshihiro Ishikawa, Yasuhiko Kohtoku, Kiyoshi Kumagawa et al. · Nature · 1998 · 445 citations
Natural Sciences, Materials Engineering, Materials Science +10
Thermal stability of SiC fibres (Nicalon�)
T. Mah, Norman L. Hecht, Dale E. McCullum et al. · Journal of Materials Science · 1984 · 331 citations
Natural Sciences, Materials Engineering, Materials Science +14