Journal of the American Ceramic Society · 2014 · 29 citations · 39 references
Natural SciencesMaterials EngineeringMaterials ScienceCeramic MaterialsCeramicsMaterials ChemistryDielectric CeramicsDielectricsElectrical Properties Of CeramicsStructural CeramicsCeramic DielectricsDielectric ConstantDielectric PermittivityElevated-temperature Material PropertiesFrequency DispersionPermittivityPhase Transitions In Dielectric CeramicsRoom-temperature Synthesis
Conventional solid‐state synthesis was used to synthesize dense and phase pure ceramics in the (1− x ) Bi 0.5 K 0.5 TiO 3 – x Bi 0.5 Na 0.5 ZrO 3 (BKT–BNZ) system. Structural characterization was done using X‐ray diffraction at both room temperature and elevated temperatures, identifying a transition from tetragonal x Bi 0.5 Na 0.5 ZrO 3 ( x BNZ, x = 0–0.10) to pseudo cubic x BNZ for x = 0.15–0.80. Dielectric properties were investigated with respect to both temperature (RT = 600°C) and frequency (1–10 6 Hz). Relaxor‐like behavior was retained for all the materials investigated, evident by the broadening of the relative dielectric permittivity peaks at transition temperatures as well as frequency dispersion at their maximum. The maximum dielectric constant at elevated temperature was found for 0.15 BNZ. Electric field‐induced strain and polarization response were also investigated for several compositions at RT and the largest field‐induced strain was observed for the 0.10 BNZ ceramics. The composition range with best performance coincides with the transition from tetragonal to cubic crystal structure.
39