Electron Backscatter Diffraction of Fresnoite Crystals Grown from the Surface of a 2BaO·TiO<sub>2</sub>·2.75SiO<sub>2</sub> Glass

Wolfgang Wisniewski, Marcus Nagel, Günter Völksch, Christian Rüssel

Crystal Growth & Design · 2009 · 61 citations · 23 references

Concepts

Abstract

A glass with the composition 2BaO·TiO 2 ·2.75SiO 2 was annealed at 810 °C for 20 h. This led to surface crystallization. Immediately at the surface of the sample, a layer of Ba 2 TiSi 2 O 8 -type fresnoite crystals (layer I), with a thickness of approximately 7 μm, oriented with the crystallographic [101]-direction perpendicular to the surface, was formed. The pole of the (001)-plane rotates randomly around the [101]-direction. It is assumed that nucleation kinetics is decisive to the direction of growth. In the next layer (layer II), the crystals are oriented with the crystallographic [001]-direction ( c -axis) perpendicular to the surface of the sample. This layer occurs at a distance of 7−60 μm from the surface. Here, crystals that are not oriented in that way hinder each other during crystal growth. At a distance > 60 μm, the orientation of the fresnoite crystals is random and is the result of volume crystallization. The main characterization method is electron backscatter diffraction/orientation imaging microscopy.

References

23