Materials Research Innovations · 2013 · 14 citations · 23 references
Natural SciencesMaterials EngineeringMaterials ScienceBuilding MaterialsGeotechnical EngineeringMechanical Behavior Of MaterialsComposite MaterialsGeosynthetic ReinforcementPorous MaterialsThermogravimetric AnalysisAmorphous StructureCuring ConditionsFly Ash-based MaterialsMechanical Properties After CuringMercury Intrusion PorosimetryPore VolumeThermogravimetric CurvesThermogravimetric Data Analysis
Alkali activated silica fume and fly ash based geopolymer (ASFG) were prepared through vibromoulding process, the optimum mix amount of silica fume and influence of different curing temperatures of room temperature (RT), 60, 80 and 210°C on the mechanical properties of ASFG were evaluated respectively. Results of mechanical properties shown silica fume could reinforce and toughen alkali activated fly ash based geopolymer, and the optimum additive amount of silica fume was 10 wt-% as the starting materials in various curing systems. The results of mercury intrusion porosimetry and scanning electron microscope showed that the smaller pore volume of ASFG decreased with increasing curing temperatures and formed amorphous porous network structure due to accelerated geopolymerisation; the weight loss decreased gradually and temperatures of weight loss improved with increasing curing temperatures derived from the increased content of bound water through the results of thermogravimetric analysis.
23