Journal of Environmental Quality · 1995 · 52 citations · 0 references
Natural SciencesChemistryEnvironmental EngineeringInorganic ChemistrySoil ChemistrySurface ScienceChemical OxidationCoatingsIron OxidesMine Waste ManagementMineral Surface ChemistrySurface OxidationHydrogen Peroxide TreatmentMicroencapsulationMicroencapsulation ProcessesMine Waste GeochemistryPyrite OxidationPyrite Oxidation In Mine WastePyrite Oxidation Suppression
Abstract Pyrite in mining waste is initially oxidized by the atmospheric O 2 , releasing acidity and Fe 2+ . At a pH below 3.5, Fe 2+ is rapidly reoxidixed by Thiobacillus ferrooxidans to Fe 3+ , which oxidizes pyrite at a much faster rate than O 2 . Commonly, the approach used in preventing pyrite oxidation in the field involves the use of limestone. This approach, however, has a short span of effectiveness because the surfaces of pyrite particles in mining waste are still exposed to the atmospheric O 2 after treatment. The objective of this study was to examine the feasibility in controlling pyrite oxidation by creating an FePO 4 coating on pyrite surfaces to block access of the atmospheric O 2 to pyritic surfaces. The coating methodology involved leaching pyrite using a chromatographic column with a 1 cm i.d. and a flow rate of 0.5 mL min −1 at 40°C with a PO 4 solution containing hydrogen peroxide (H 2 O 2 ); when this solution reached pyrite surfaces, H 2 O 2 oxidized the surface portion of pyrite and released Fe 3+ so that Fe phosphate precipitated and formed a passive coating on pyritic surfaces. This laboratory‐scale study demonstrated that Fe phosphate coatings on pyritic surfaces could be established with a solution containing as low as 10 −4 tool L −1 phosphate and 0.03 mol L −1 H 2 O 2 and that the FePO 4 phosphate coating could effectively protect pyrite from oxidizing further.