Journal of Vacuum Science & Technology A Vacuum Surfaces and Films · 1987 · 22 citations · 0 references
Natural SciencesChemistryMaterials ScienceCorrosion ScienceSurface ChemistrySurface ScienceAluminum HydroxidesAluminum OxidesCorrosion EngineeringCorrosion KineticsCorrosion MechanismsElectrochemical CorrosionAluminum CorrosionAnodic PolarizationCorrosion In Acidic MediaCorrosion PotentialEquilibrium ConditionsOxide Film FormationPh-dependent Corrosion BehaviorPourbaix Diagrams
The composition and thickness of the oxide/hydroxide film that forms on pure Al polarized in 0.05M Na2SO4 solutions with and without the addition of 1000 ppm Cl− under acidic, near-neutral, and alkaline conditions have been determined using x-ray photoelectron spectroscopy. Changes in the films due to the ex situ nature of the measurements have also been characterized. The results were plotted on surface behavior diagrams to follow the evolution of the surface during polarization and compared with the results predicted by the Pourbaix diagram. Although Al(OH)3 is the most stable species to form in near-neutral solutions under equilibrium conditions, the composition of the film at the corrosion potential under our experimental conditions was found to be that of the oxyhydroxide AlOOH at each pH. In the pH 7 and pH 10 solutions, this film thickens during anodic polarization (up to the pitting potential for the Cl−-containing solutions), but the composition is unchanged. In contrast, the Cl−-free, pH 2 solutions, an oxide film forms at the oxyhydroxide–metal interface and rapidly thickens with increasing anodic overpotentials. The original AlOOH layer then slowly dissolves so that the film becomes entirely Al2O3. During cathodic polarization, we observed growth of the oxyhydroxide film, especially at pH 2, which we attributed to cathodic corrosion.