Synthesis of <i>exo</i>-Olefin Terminated Polyisobutylene by Sulfide/Base Quenching of Living Polyisobutylene

Subramanyam Ummadisetty, David L. Morgan, Casey D. Stokes, Robson F. Storey

Macromolecules · 2011 · 46 citations · 16 references

Concepts

Abstract

exo -Olefin (methyl vinylidene)-terminated polyisobutylene (PIB) was synthesized in one pot by quenching TiCl 4 -catalyzed living PIB with a dialkyl (or) diaryl sulfide at −60 to −40 °C, followed by addition of a base ( e.g ., triethylamine), followed by warming of the reaction mixture to −20 to −10 °C and final termination with methanol. The initiator was 2-chloro-2,4,4-trimethylpentane (TMPCl); the solvent system was 60/40 hexane/methyl chloride, and 2,6-lutidine was used as a nucleophilic additive during polymerization. 1 H NMR spectroscopy was used characterize end-group composition of the product PIBs. Increasing yield of exo -olefin end groups was observed in the approximate order of increasing bulkiness of the substituent on the sulfide, i.e ., tert -butyl (100%) > isopropyl (98%) > phenyl (70%) > n -alkyl (39–55%). With diisopropyl sulfide (DIPS), optimized yield of exo -olefin (98%) required stoichiometric excess of DIPS relative to chain ends (CE), e.g., [DIPS]/[CE] = 4, addition of a base, and warming of the reaction prior to addition of methanol. With di- tert -butyl sulfide (D t BS), optimized yield was obtained with lesser stoichiometric excess, e.g., [D t BS]/[CE] = 1.5, with or without addition of a base, and with or without warming of the reaction prior to methanol termination. D t BS yielded 100% exo -olefin end groups under concentrated conditions, e.g., [CE] = 0.1 M, and 98% exo -olefin when the reaction was up-scaled to produce 0.8 kg of PIB. The method was successfully adapted to the synthesis of telechelic (difunctional) exo -olefin terminated PIB with quantitative functionality (100%).

References

16