CORROSION · 1983 · 16 citations · 4 references
Natural SciencesMaterials EngineeringMaterials ScienceCorrosion ScienceMaterials CharacterizationMechanical Behavior Of MaterialsCorrosion EngineeringCorrosion KineticsCorrosion MechanismsCorrosion TestingCorrosion-resistant MaterialsStress Corrosion CrackingCorrosion AssessmentCrack GrowthCrack Growth MeasurementCrack Growth RateCrack Growth TestingElectrolytesStress Corrosion Cracking Testing
Double cantilever beam specimens were employed to measure the rate of stress corrosion crack growth of AA 7075-T651 in 1 N NaClO4, 1 N NaCl, 1 N Na2SO4, and 1 N NaNO3 solutions. Perchlorate is a noncomplexing anion, so the tests conducted in NaClO4 solution should not be affected by specific anion effects. The data were treated statistically to arrive at a measure of the reliability of the test using DCB specimens. The crack growth rate in 1 N NaClO4 solution was 0.81 × 10−6 cm sec−1, as compared with 1 N NaCl solution, 1.43 × 10−6 cm sec−1; 1 N NaNO3, 0.48 × 10−6 cm sec−1; and Na2SO4, 0.29 × 10−6 cm sec−1. These tests are generally reproducible to about 5 to 10%. The pH of the solution in the advancing crack in NaClO4 solution was 6.2 to 6.9, as compared with 3.2 in NaCl solution. The Al+++ concentration was low, in the range of 0.005 to 0.001 M. To study metallurgical effects in the stress corrosion cracking of high strength aluminum alloys, it would be advisable to use perchlorate instead of chloride solutions to avoid specific anion effects.
4