Science and Technology of Welding & Joining · 2006 · 103 citations · 4 references
EngineeringMaterials EngineeringMaterials ScienceMechanical Behavior Of MaterialsMetallic MaterialsMetallurgyAlloysGrain Structure FormationMetalsPhysical MetallurgySteel MaterialsWeldingBainite FormationMartensitic MicrostructureMicrostructureSegregationSteel MicrostructureToughnessWeld Metal MicrostructureWeld Microstructure
The effects of increasing the nickel content from 3 to 7 or 9 wt-% were investigated in high strength steel weld metals with 2 wt-% manganese. Nickel additions were beneficial to strength but detrimental to impact toughness. Significant segregation of nickel and manganese to interdendritic regions was observed at the two higher nickel contents. In these weld metals a mainly martensitic microstructure developed at interdendritic regions, whereas bainite was found at dendrite core regions. The microstructural inhomogeneity was due to segregation and the accompanying stabilisation of austenite in solute enriched regions to lower transformation temperatures. With 3 wt-% nickel the microstructure was found to be more homogeneous, with mainly bainite forming. The decrease in impact toughness with increasing nickel content was mainly attributed to the formation of coarse grained coalesced bainite.
4
E. Keehan, Leif Karlsson, H.-O. Andrén et al. · Science and Technology of Welding & Joining · 2006 · 71 citations
Natural Sciences, Materials Engineering, Materials Science +17
E. Keehan, Leif Karlsson, H.-O. Andrén et al. · Science and Technology of Welding & Joining · 2006 · 63 citations