IBM Journal of Research and Development · 1966 · 10 citations · 3 references
Natural SciencesMaterials EngineeringMaterials ScienceElectronic MaterialsMagnetic MaterialsThin FilmsMemory DevicesThin Film Thermal PropertiesFilm StressMagnetic RecordingMemory CapacityMemory Storage CapacityStressTemperature Gradient EffectsThermomechanical Stress
Where the magnetostrictive coefficient is of the order of 10 <sup xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">−6</sup> or greater, recording may be accomplished on uniaxial Permalloy films by the application of a local stress in coincidence with a biasing field. Here, the stress is introduced into the film as a result of a temperature gradient produced by an incident laser or electron beam. The mechanism of recording is studied and a model developed in agreement with the mechanism. Several modes of recording are discussed, with the advantages and disadvantages of each. Extrapolating the model to a large capacity memory of 10 <sup xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">7</sup> bits per square inch with 8 micron diameter spots on a Permalloy film having a magnetostrictive coefficient of 10 <sup xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">−5</sup> , a 20°C temperature rise will be experienced with 2 × 10 <sup xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">−10</sup> joules of energy in the beam. The beam power required is 10 <sup xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">−3</sup> watts at 10% efficiency and a one megacycle information rate.
3