Macromolecules · 2010 · 57 citations · 71 references
Natural SciencesChemistryMaterials SciencePolymer ChemistryPolymer EngineeringPolymer MaterialsPolymer MorphologyPolymer Phase BehaviorPolymer Physical ChemistryPolymer StructurePolymeric NanomaterialsPolymerization ChemistryAtom Transfer Radical PolymerizationBrushesControlled Radical PolymerizationMicrophase SeparationNitroxide-mediated PolymerizationPolymer BrushesPolystyreneSurface-initiated Polymerization
We report in this article the synthesis of a series of mixed poly( tert -butyl acrylate) (P t BA)/polystyrene (PS) brushes with P t BA number-average molecular weight ( M n ) being fixed at 24.5 kDa and PS M n ranging from 14.8 to 30.4 kDa on 160 nm silica particles and the study of their microphase separation behaviors using differential scanning calorimetry (DSC) and transmission electron microscopy (TEM). The samples were synthesized by a two-step “grafting from” process from asymmetric difunctional initiator (Y-initiator)-functionalized silica particles using two different “living”/controlled radical polymerization techniques. P t BA brushes were grown first from Y-initiator-functionalized particles by surface-initiated atom transfer radical polymerization of tert -butyl acrylate at 75 °C in the presence of a free initiator, followed by nitroxide-mediated radical polymerization (NMRP) of styrene at 120 °C. The “living” nature of NMRP allowed the synthesis of mixed P t BA/PS brushes with different PS molecular weights (14.8, 18.7, 24.9, and 30.4 kDa) in a one-pot polymerization. DSC studies showed that all thermally annealed mixed brush samples exhibited two glass transitions with the middle points located at ∼47 and ∼90 °C, suggesting that the two tethered polymers microphase separated in the brush layer. For TEM studies, the samples were dispersed in CHCl 3, a good solvent for both P t BA and PS, drop-cast onto carbon films, thermally annealed in vacuum at 120 °C for 3 h, and then stained with RuO 4 vapor. All samples showed clear microphase separation, consistent with the DSC results. With increasing PS M n from 14.8, to 18.7, and 24.9 kDa, the morphology of mixed brushes evolved from isolated, nearly spherical PS microdomains buried inside the P t BA matrix, to short PS cylindrical microdomains in the P t BA matrix, and to nearly bicontinuous nanostructures. Further increasing the molecular weight of PS to 30.4 kDa resulted in the formation of isolated P t BA microdomains which were covered by PS chains.
71
Polymer brushes: surface-immobilized macromolecules
Bin Zhao, William J. Brittain · Progress in Polymer Science · 2000 · 1.6K citations
Polymer-Polymer Phase Behavior
Frank S. Bates · Science · 1991 · 1.4K citations
Natural Sciences, Materials Engineering, Materials Science +17
Physical properties of polymers handbook
Choice Reviews Online · 1996 · 1K citations