Degradation of Y<sub>2</sub>O<sub>3</sub>-Stabilized ZrO<sub>2</sub> Ceramics in Artificial Saliva: ICP Analysis of Dissolved Y<sup>3+</sup> and Zr<sup>4+</sup> Ions

L.E. Mukaeda, Simone Pereira Taguchi, A. Robin, H.J. Izario, Claudinei dos Santos

Materials science forum · 2012 · 13 citations · 6 references

DOIFull text

Open access

Concepts

Abstract

ZrO 2 ceramics are one of the most important materials used in dental prostheses production, due to their excellent mechanical resistance and chemical inertness in the mouth environment. Nevertheless, the combination of low pHs and fluoride presence is able to reduce the chemical stability of these ceramics. In this work, the resistance of commercial blocks of micrometric and nanometric sized Y 2 O 3 -stabilized ZrO 2 ceramics (ProtMat Materiais Avançados® and Ivoclar®) was evaluated in Fusayama artificial saliva of different pHs with (and without) the presence of fluoride ions. The study was based on the analysis of the amount of Zr 4+ and Y 3+ ions dissolved in the artificial saliva after different exposure times using ICP OES technique. The XRD technique was also employed to investigate the phase transformations occurring during the degradation process in artificial saliva. The micrometric sized ZrO 2 ceramics presented higher resistance in the artificial saliva than nanometric sized structures.

References

6